cover
Zandini Nurichi
" Fabricate through-hole porous anodic aluminum oxide (AAO) template were made by a two-step anodization method of an aluminum with purity 99,98% in 0,3 M oxalic acid at 45 V with 360 minutes of second anodization time. The effect of duration time on the second anodizing step, voltage and solution of the electrolyte on the porous oxide layer and influence of the pore opening on the structural as a template were studied in detail. Then, the ... "
Depok: Universitas Indonesia, 2016
S64000
UI - Skripsi Membership  Universitas Indonesia Library
cover
Fara Dewi Syamdri
" Fabrikasi templet Anodic aluminium Oxide AAO sebagai nanoporous dilakukan dengan proses anodisasi dengan metode two-step anodization menggunakan alumunium dengan kemurnian 99,98 dengan variasi larutan elektrolit yaitu, larutan asam oksalat dan asam sulfat dengan variasi konsentrasi 0,3 M untuk asam oksalat dan 0,1 M, 0,3 M dan 0,5 M untuk asam sulfat, serta waktu anodisasi kedua sebesar 360 menit. Waktu anodisasi, larutan dan konsentrasi elektrolit, serta arus yang digunakan menjadi faktor utama dalam pembentukan ketebalan lapisan ... "
Depok: Universitas Indonesia, 2017
S69435
UI - Skripsi Membership  Universitas Indonesia Library