Anne Zulfia
" Pure Al/SiC metal matrix composites (MMC) have been successful produced by the Lanxide process with different processing temperature for 8 hours. The process is simply without aid externally pressure. However, N2 oxygen free was flushed during the process. Molten pure Al has fully infiltrated to the preform with Sl/1% Mg at 750, 800, 850, 900 and 1000°C§ but infiltration did not occur to the preform with 3Vj'% Mg. Voids exist above the infiltrated preform in ... "
Depok: Fakultas Teknik Universitas Indonesia, 2001
JUTE-15-2-Jun2001-202
Artikel Jurnal  Universitas Indonesia Library